Warm glass kiln firing schedule for slumping. Enter these steps into your kiln.
Step 1: to 1000°
Step 2: to 1450°
Step 3: 1450°
Step 4: to 980°
Step 5: @ 980°
Step 6: to 875°
Step 7: @ 875°
Step 8: to 775°
Step 9: @ 775°
Step 10: Off