Warm glass kiln firing schedule for Tack Fusing. Enter these steps into your kiln.
Step 1: 2 Hrs. to 1350° F
Step 2: 1/2 Hr. @ 1350° F
Step 3: 1 minute to 980° F
Step 4: 1/2 Hr. @ 980° F
Step 5: 1 minute to 875° F
Step 6: 1/2 Hr. @ 875° F
Step 7: 1 minute to 775° F
Step 8: 1/2 Hr. @ 775° F
Step 9: Turn Kiln Off